Case study for Gypsum screening (moisture 3.3%, cut point 600 microns)
Kroosh Technologies Ltd

Case study for Gypsum screening (moisture 3.3%, cut point 600 microns)

The customer uses gypsum to produce dry mix mortars. The product's moisture didn't allow another screeners to screen the product at 0.6mm cut point. KROOSH successfully solved this difficult task.

Share:

Facebook
Twitter
LinkedIn
WhatsApp

Purpose: screening of gypsum with moisture 3.3% at cut 0.6mm.
Application: gypsum plants or dry mortars plants.
Product: gypsum cut point 0.6 мм
KROOSH Results: on-spec screening of hard-to-screen product with high moisture.